Welding Journal · 1994 · 27 citations · 0 references
EngineeringManufacturing EngineeringMaterials EngineeringConstruction TechnologyMetallurgyProduction EngineeringLaser Beam WeldingSpot WeldingWeldingWelding ProcessesWeld MicrostructureWeld Quality AssessmentWeld Quality ControlWelding Metallurgy Of SteelsWelding Process Parameters
The effects of temporal pulse shape on weld dimensions and weld quality of Nd:YAG laser spot welds produced in AISI 304 stainless steel have been examined over a range of power densities and pulse times. Four different temporal pulse types were used: normal rectangular'' pulses with a characteristic leading-edge power spike, rectangular pulses with no spike, ramped-up pulses and ramped-down pulses. Pulse shaping had no significant effect on the weld dimensions or weld quality of the conduction-mode welds. Removal of the leading-edge power spike from rectangular'' pulse shapes tended to reduce the weld diameter and crater area of keyhole-mode welds, but had little effect on other measures of size or quality. However, the diameter, penetration and melt area of keyhole-mode welds made with ramped-up or ramped-down pulse shapes were consistently greater than those made with the rectangular pulse shape. Also, the penetration and melt area of keyhole-mode welds made with the ramped-up pulse shape were greater than those made with the ramped-down pulse shape. Keyhole-mode welds made with ramped-up pulse shapes had the greatest occluded gas porosity, but the smallest crater areas. Alternatively, welds made with the ramped-down pulse shape exhibited the least porosity, but the greatest crater areas.