Journal of Prosthodontics · 2014 · 70 citations · 28 references
DentistryDental Biomaterials ScienceDental Materials ScienceDental MaterialsProsthodontic MaterialsSurface Properties Of Dental MaterialsCeramic RestorationsCrown MaterialsDental CeramicsTooth FormCeramic Crown SystemsCrown Fabrication MaterialsIn Vivo StudiesLaser Surface MeltingLithium Disilicate CrownsMetal-ceramic Crown Marginal FitSelective Laser Melting
PURPOSE: The aims of this in vivo investigation were to compare the marginal and internal fit of single-unit crowns fabricated using a selective laser melting (SLM) procedure with two CAD/CAM grinding procedures, and to evaluate the influence of tooth type on the parameters measured. MATERIALS AND METHODS: A total of 270 crowns were evaluated, including 90 SLM metal-ceramic crowns (group B), 90 zirconium-oxide-based ceramic crowns (group L), and 90 lithium disilicate ceramic crowns (group C). The marginal and internal gaps of the crowns were recorded using a replica technique with a silicone indicator paste stabilized with a light-body silicone. The gap replica specimen were sectioned buccolingually and mesiodistally and then examined using a stereomicroscope at 30× magnification. Ten reference points were measured on each anterior and premolar specimen, and 20 reference points were measured on each molar specimen. Two-way ANOVA was performed to identify the significant differences between the groups. RESULTS: The mean marginal fit of group B was significantly better than those of group C and group L (p < 0.005), but a significant difference was not found between group C and group L (p > 0.05). The mean axial gap of group B was significantly smaller than those of group C and group L (p < 0.01), while group C was not different from group L (p > 0.05). The mean occlusal gap of group B was significantly higher than those of group C and group L (p < 0.05), and no difference was found between group C and group L (p > 0.05). The marginal and internal gaps of crowns varying according to tooth type were not significantly different (p > 0.05). CONCLUSION: The SLM system demonstrated better marginal and internal fit compared to the two CAD/CAM grinding systems examined. Tooth type did not significantly influence the marginal or internal fit.
28
The estimation of cement film thickness by an in vivo technique
J W McLean, Fraunhofer von · BDJ · 1971 · 1.4K citations
Marginal fit of gold inlay castings
Gordon J. Christensen · Journal of Prosthetic Dentistry · 1966 · 429 citations
Clinical fit of Procera AllCeram crowns
Klaus Boening, Burkhard H. Wolf, Annette Schmidt et al. · Journal of Prosthetic Dentistry · 2000 · 286 citations