Materials Transactions JIM · 2000 · 72 citations · 11 references
Natural SciencesMaterials EngineeringMaterials ScienceMagnetic MaterialsMetallic MaterialsMetallurgyAlloysAmorphous Magnetic MaterialsAmorphous MaterialsAmorphous SolidsCurie TemperatureMagnetic Properties Of SolidsAmorphous AlloysAmorphous Magnetic AlloysAmorphous MetalsGlass TransitionGlass Transition TemperatureMagnetic AlloysMagnetic PropertiesMold Casting
Amorphous Fe75Ga5P12C4B4 alloy rods were prepared in the diameter range up to 1.0 mm by copper mold casting. The glass transition temperature (Tg), supercooled liquid region (ΔTx(=Tx−Tg)) and reduced glass transition temperature (Tg⁄Tm) of the amorphous alloy rods are 731 K, 37 K and 0.61, respectively, in agreement with the results for the corresponding melt-spun amorphous alloy ribbon. The Curie temperature (Tc), saturated magnetization (Is), coercive force (Hc) and saturated magnetostriction (λs) of the melt-spun amorphous ribbon are 622 K, 1.28 T, 1.6 A/m and 19.6×10−6, respectively, in which the Tc and Is are nearly the same as those for the amorphous alloy rod with a diameter of 0.5 mm. The simultaneous achievement of high Tg⁄Tm, large ΔTx and good soft magnetic properties for the simple Fe-based alloy system is promising for the future development of bulk amorphous Fe-based soft magnetic alloys.
11
Stabilization of metallic supercooled liquid and bulk amorphous alloys
Akihisa Inoue · Acta Materialia · 2000 · 5.8K citations