Effect of an increase in opening roller width on quality of rotor spun yarn

Babak Yadollah Roudbari, Safdar Eskandarnejad, M. Bameni Moghadam

Journal of the Textile Institute · 2015 · 17 citations · 8 references

Concepts

Abstract

Opening of fibres by opening roller (OR) in rotor spinning is one of the most influential parameters on yarn quality. In order to increase working surface of the OR, its width was increased by 25 and 50% with respect to the original width and nine samples of yarn were produced. Yarn properties tested were tenacity, strain at peak, work of rupture, evenness, imperfections, hairiness and fibre extent within the yarn structure. It was concluded from the test results that, an increase in fibre opening in lower level improves yarn quality. However, further increase in amount of fibre opening at higher level improves the quality up to a certain point, and then it deteriorates. Yarn sample B8 was the best yarn produced and was superior to the rest of the yarns.

References

8