Origin of Conductivity Threshold in the Solid Electrolyte Glass System: $( \hbox{Ag}_{2} \hbox{S})_{x}( \hbox{As}_{2} \hbox{S}_{3})_{1-x}$

Chad Holbrook, Ping Chen, D. Novita, P. Boolchand

IEEE Transactions on Nanotechnology · 2007 · 13 citations · 17 references

Concepts

Abstract

The electrical conductivity of (Ag <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sub> S) <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">x</sub> (As <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sub> S <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">3</sub> ) <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">1-x</sub> glasses increases to display a step-like jump of nearly five orders of magnitude in the narrow composition range, 9% < x < 15% range. To elucidate the origin of this threshold behavior, we have now examined the molecular structure of these glasses in modulated-differential scanning calorimetry (MDSC) and Raman scattering experiments. Our MDSC results reveal bimodal glass transition temperatures (T <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">g</sub> s), a low-T <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">g</sub> and a high-T <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">g</sub> in the 7% < x < 40% range but unimodal ones outside this range. The low-T <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">g</sub> phase bears a similarity to that of the stoichiometric glass at x = 1/2, or AgAsS <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sub> , and we identify it with a Ag-rich phase formed in these glasses once x > 7%. The Ag-rich phase is thought to percolate near x ~ 9%, and to contribute to the large jump in conductivity of the glasses. The high-Tg phase represents a semiconducting As <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sub> S <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">3</sub> glass phase alloyed with a few mole percent of Ag <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sub> S, and it displays a reversibility window in the 8% < x < 13% range. The semiconducting phase becomes elastically flexible once x > 13%. Softening of the high-Tg phase lowers Ag <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">+</sup> ion migration energies and also contributes to the conductivity threshold.

References

17