STABILIZATION OF HEAVY METALS IN PORTLAND CEMENT, SILICA FUME/PORTLAND CEMENT AND MASONRY CEMENT MATRICES

JI Bhatty, F.M. Miller, P B West, Bernhard Ost

1999 · 16 citations · 8 references

Concepts

Abstract

The effects of heavy metals on the physical and chemical properties of portland-cement based pastes were studied using different types of cement, four metal oxides, and four soluble metal salts. Type I (high calcium aluminate content) and Type V (low calcium aluminate content) portland cements were used to study the effects of their chemical differences on paste properties and metal stabilization. Fresh pastes were tested for workability, initial setting times, and heats of hydration. Hardened pastes were tested for strength and leachability by both TCLP (Toxic Characteristic Leaching Procedure) and column leaching with acetic acid. The cement matrix was an excellent stabilization matrix, better than could be projected from pH considerations alone. The investigation also involved examining Type I portland cement paste treated with three metals together - chromium, cadmium and lead, added at very high (1% by mass of cement) and intermediate (1000 ppm by mass of cement) levels. The leaching solutions were acetic acid, synthetic rain (pH 3 sulfuric/nitric acid), and deionized water. A Type N masonry cement matrix was also investigated. The leachabilities were very low throughout the pH range of 6-11 for lead and chromium. At very high pH values, the leachabilities of lead and chromium were significantly higher. Cadmium leachability was negligible above pH 10, but became rapid and highly significant below pH 9. At pH values below 6, which generally corresponded to the extraction of nearly all calcium present, all metals were rendered highly leachable. For all the metals, the leachability in masonry cement-stabilized matrix has higher than with Type I during the intermediate leaching steps. A series of tests involved testing of a contaminated soil matrix, both dry and contaminated with aged SAE 10 W oil (without additives). Cement was used at 8% by weight of total mix. The results of leachability vs pH generally were consistent with those obtained in the multiple metals leaching studies; as long as calcium silicate hydrate was present, metals solubility was very low, irrespective of pH. In an attempt to address the early high pH leaching of lead and chromium, a series of experiments was run with silica fume, in an amount calculated to react with all calcium hydroxide generated from hydration of the calcium silicates. The results indicated that leachabilities of lead and chromium were reduced at pH values greater than 11.0, and also at the low pH values obtained after multiple sequential batch leaches. Since ettringite is known to be much less soluble than calcium monosulfoaluminate hydrate, it was also though that a system in which extra sulfate is present might yield even lower leachabilities for those metals which were substituted in the ettringite lattice. The results indicated that at very high pH values, the leachability of chromium was reduced with the lower excess gypsum level, and at low pH values, less than about 5.0, with both high gypsum levels. At intermediate pH values, chromium leachability was minimum for the unaltered matrix.

References

8